Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 16 hour | 16 hour | F50; ASTM D1693B |
SABIC BM6246LS High Density Polyethylene for Blow Molding Product Description: BM6246LS grade is a medium molecular weight High Density Polyethylene homopolymer for blow molding applications. It is primarily designed for imparting high rigidity, toughnes.. |
|||
ESCR 10% Igepal® | 16 hour @Thickness 2.00 mm, Temperature 50.0 °C |
16 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem GD5160 HDPE Blow Molding Polyethylene Homopolymer GD5160 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance and productivity. It was developed for the blow-molding segment. It is used in .. |