Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | >= 360 hour @Temperature 50.0 °C |
>= 360 hour @Temperature 122 °F |
F<sub>50</sub>; ASTM D1693 |
Westlake EMAC® SP 1205 Ethylene-Methyl Acrylate Copolymer
(discontinued **) 20% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing up to .. |
|||
ESCR 10% Igepal® | >= 360 hour @Temperature 50.0 °C |
>= 360 hour @Temperature 122 °F |
F<sub>50</sub>; ASTM D1693 |
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer
(discontinued **) 20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows .. |