Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 30 hour @Temperature 50.0 °C |
30 hour @Temperature 122 °F |
ASTM D1693B |
ExxonMobil LLDPE LL 6301RQ Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra.. |
|||
ESCR 10% Igepal® | 30 hour @Temperature 50.0 °C |
30 hour @Temperature 122 °F |
ASTM D1693B |
ExxonMobil LLDPE LL 6301XR Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra.. |
|||
ESCR 10% Igepal® | 30 hour @Thickness 1.91 mm |
30 hour @Thickness 0.0750 in |
F50; ASTM D1693 |
ExxonMobil LLDPE LL 8446.21 Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 8446 is a linear low density butane copolymer designed to offer excellent processability, whiteness, and fast grinding rate. This UV stabilized resin is ideally suited for ap.. |