Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F50; ASTM D1693 |
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b.. |
|||
ESCR 10% Igepal® | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F<sub>50</sub>; Condition A, From compression molded specimens; ASTM D1693 |
NOVA Chemicals Sclair® 8107 UV8D Butene LLDPE Rotational Molding Resin Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693-B |
Petromont 1202 High Density Polyethylene Resin Petromont HDPE 1202 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as shipping containers.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693-B |
Petromont 4100 High Density Polyethylene Resin Petromont HDPE 4100 is a high density polyethylene copolymer resin produced using the UNIPOL®
Process. This resin is designed for general use in large diameter heavy duty and non pressure pipe
appl.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693-B |
Petromont 5001 High Density Polyethylene Resin Petromont HDPE 5001 is a high-density polyethylene copolymer resin produced using the UNIPOL®
Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
ESCR 10% Igepal® | 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
ESCR 10% Igepal® | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F<sub>50</sub>; Condition A, From compression molded specimens; ASTM D1693 |
NOVA Chemicals Sclair® 8107G UV8D Butene LLDPE Rotational Molding Resin Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables Superclean LR4201S is a Superclean crosslinkable low density polyethylene (XLPE) for medium and high voltage power cable insulation. The formulation of LR4201S provides an optimum combination of go.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693 |
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | Condition B, F50; ASTM D1693 |
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade This hexene copolymer is tailored for pipe applications that require:Good melt strengthGood pipe stiffnessOutstanding ESCRTypical corrugated pipe applications for HP076 include:Culverts and storm se.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693A |
ExxonMobil Paxon™ 7003 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693A |
ExxonMobil Paxon™ 7004 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693A |
ExxonMobil Paxon™ 7203 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693A |
ExxonMobil Paxon™ 7204 Crosslinkable Rotational Molding Resin Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite.. |
|||
ESCR 10% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693, B |
Total Lumicene® mPE BM359 SG Metallocene Medium Density High Gloss Blow Molding Resin Metallocene Medium Density High Gloss Blow Molding ResinCharacteristics:Outstanding glossGood flexibilityExcellent impact strengthGood ESCRUSP Class VI compliantFDA CompliantApplications:Coextruded .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
ESCR 10% Igepal® | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/370 Polyolefin, Unspecified
(discontinued **) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |