Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | >= 150 hour | >= 150 hour | F50; ASTM D1693B |
SABIC R40039E Medium Density Polyethylene for Rotational Molding Product Description: R40039E is a Medium Density Polyethylene grade designed to provide excellent mechanical properties with high rigidity, toughness, gloss and low warpage. R40039E is UV stabiliz.. |
|||
ESCR 100% Igepal® | >= 150 hour | >= 150 hour | F50; ASTM D1693B |
SABIC R50035 Linear Low Density Polyethylene for Rotational Molding Product Description: R50035 are Linear Low Density Polyethylene grades designed to provide excellent stress crack resistance, mechanical properties with high rigidity, toughness, gloss and low warp.. |
|||
ESCR 100% Igepal® | 150 hour @Thickness 3.80 mm, Temperature 23.0 °C |
150 hour @Thickness 0.150 in, Temperature 73.4 °F |
slit; ASTM D1693 |
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin
(discontinued **) LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance,.. |
|||
ESCR 100% Igepal® | >= 150 hour | >= 150 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HP5221 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP5221 is a high performance copolymer that is designed for the most demanding requirements of corrugated pipe applications. Formolene® HP5221 meets the re.. |
|||
ESCR 100% Igepal® | >= 150 hour | >= 150 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® E602 Pipe HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E602 is a high performance copolymer that is designed for the most demanding r.. |