Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 50 hour | 50 hour | Conditions A and B; ASTM D1693 |
Chevron Phillips Marlex® HHM 5202LD HDPE Blow Molding Resin
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good stiffnessExceptional processabilityGood ESCRApplications: Household & industrial chemical containersInformation provided by Chevron Phillips. |
|||
ESCR 100% Igepal® | >= 50 hour | >= 50 hour | Condition C; ASTM D1693 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition C; ASTM D1692 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
ESCR 100% Igepal® | >= 50 hour | >= 50 hour | Condition C; ASTM D1693 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition C; ASTM D1692 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition A, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5202A Blow Molding HDPE High Density Polyethylene Hexene Copolymer for Blow Molding – With Antistat Formolene® HB5202A is designed for applications requiring excellent stiffness and stress crack resistance propertiesAppl.. |
|||
ESCR 100% Igepal® | >= 50 hour | >= 50 hour | Condition C; ASTM D1693 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
ESCR 100% Igepal® | >= 50 hour | >= 50 hour | Condition C; ASTM D1693 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition C; ASTM D1692 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
ESCR 100% Igepal® | >= 50 hour | >= 50 hour | Condition C; ASTM D1693 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition C; ASTM D1692 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition C; ASTM D1692 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition C; ASTM D1692 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition B, F50; ASTM D-1693 |
Chevron Phillips Marlex® 9514H Polyethylene; HDPE High density polyethylene. This gas phase, high molecular weight hexene copolymer is tailored for lightweight blow molded applications that: Require excellent stiffness to ESCR ratioRequire good m.. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | F50; ASTM D1963 |
ExxonMobil HDPE HYA 600 High Density Polyethylene Resin Product Description: HYA 600 is a general purpose HDPE resin, characterized by very easy processability, an excellent balance of rigidity and impact strength and a good ESCR.Availability: Africa & M.. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition A, F<sub>50</sub> CO-630; ASTM D1693 |
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition A, F<sub>50</sub> CO-630; ASTM D1693 |
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
ESCR 100% Igepal® | 50 hour @Temperature 50.0 °C |
50 hour @Temperature 122 °F |
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693 |
Dow UNIVAL™ DMDD-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6200 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package hous.. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition A, F50; ASTM D1693 |
Amco PRIMATOP HDPE 003952 Phillips Process Hexene Copolymer HDPE 003952 features excellent stiffness and stress crack resistance properties. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco produ.. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition B, F50; ASTM D1693 |
Amco PRIMATOP HDPE 003952 Phillips Process Hexene Copolymer HDPE 003952 features excellent stiffness and stress crack resistance properties. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco produ.. |
|||
ESCR 100% Igepal® | >= 50 hour | >= 50 hour | Condition C; ASTM D1693 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
ESCR 100% Igepal® | 50 hour | 50 hour | Condition B, F50; ASTM D1693 |
Chevron Phillips Marlex® 9515H High Density Polyethylene, Blow Molding This gas phase, high molecular weight, hexane copolymer with antistatic agent is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt str.. |