Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 196 cm³/g | 196 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity Test | 196 cm³/g | 196 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F130-C PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity Test | 196 cm³/g | 196 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F130-C2 PA6 Medium Viscosity, Film Extrusion, Lubricated |
|||
Viscosity Test | 196 cm³/g | 196 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F130-C3 PA6 Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated |