Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 150 cm³/g | 150 cm³/g | Average value: 150 cm³/g Grade Count:3 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Viscosity Test | 150 - 250 cm³/g | 150 - 250 cm³/g | Average value: 203 cm³/g Grade Count:9 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F6 Nylon 6, 30% Glass Fiber SAXAMID 126F6 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Other properties are .. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F6RY01 Nylon 6, 30% Glass Fiber SAXAMID 126F6RY01 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F6T3 Nylon 6, 30% Glass Fiber and PTFE SAXAMID 126F6T3 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers and 15% PTFE. Because of its high strength and stiffness this grade is often used for stressed parts requiri.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F8 Nylon 6, 40% Glass Fiber SAXAMID 126F8 is a polyamide 6 injection-molding-grade reinforced with 40% glass fibers.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226 Nylon 6.6 SAXAMID 226 is a general purpose polyamide 6.6 injection-molding-grade. Benefits are short cycle times and good release properties.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F4 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F5RY01 Nylon 6.6, 25% Glass Fiber SAXAMID 226F5RY01 is a polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has a halogen-free flame retardant and UL listed.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F7 Nylon 6.6, 35% Glass Fiber SAXAMID 226F7 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 35% glass fibers. It has very high mechanical strength in combination with good impact resistance. It is char.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F5 Nylon 6, 25% Glass Fiber SAXAMID 126F5 is a polyamide 6 injection-molding-grade reinforced with 25% glass fibers.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 73G15HSL BK363 Nylon 6
(Unverified Data**) 15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G15HSL BK363 is a 15% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applic.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® RS LC3060 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Medium Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3060 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewable sourced ingredi.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® B3K PA6 (Conditioned) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number |
BASF Ultramid® B3S Q661 PA6 (Dry) Ultramid B3S Q661 is a general purpose, PA6 resin for injection molding. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® B3K PA6 (Dry) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number |
BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry) Ultramid B3M6 is a 30% mineral reinforced injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent laser markability. |