Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 76 - 80 cm³/g | 76 - 80 cm³/g | ZIMMER WN-B010-7040E |
Iran Petrochemical (PCC) PET BG-781 Polyethylene Terephthalate Polyethylene Terephthalate bottle grade chips (highly viscous ) is a condensation polymer produced by a continuous meltphase polymerization process followed by a solid state polymerization process. .. |
|||
Viscosity Test | 76 - 80 cm³/g | 76 - 80 cm³/g | Ubbelhode |
Iran Petrochemical (PCC) PET BG-785 Polyethylene Terephthalate Polyethylene Terephthalate, bottle gradeApplications: mineral water, edible oil, small jarsInformation provided by Iran Petrochemical Commercial Co. |
|||
Viscosity Test | 76 - 80 cm³/g | 76 - 80 cm³/g | ZIMMER WN-B010-7040E |
Iran Petrochemical (PCC) PET BG-800 Polyethylene Terephthalate Polyethylene Terephthalate bottle grade chips (highly viscous ) is a condensation polymer produced by a continuous meltphase polymerization process followed by a solid state polymerization process. .. |