Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 63 - 65 cm³/g | 63 - 65 cm³/g | Ubbelhode |
Iran Petrochemical (PCC) TG 641 Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chips, semi dullApplications: staple fiber, textile filament, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co. |
|||
Viscosity Test | 63 - 65 cm³/g | 63 - 65 cm³/g | Ubbelhode |
Iran Petrochemical (PCC) TG 641 Super Bright Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chips, super brightApplications: staple fiber, textile filament, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co. |
|||
Viscosity Test | 63 - 65 cm³/g | 63 - 65 cm³/g | Ubbelhode |
Iran Petrochemical (PCC) TG 645 Super Bright Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chips, super brightInformation provided by Iran Petrochemical Commercial Co. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity Number |
Mitsubishi Xantar® 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity Number |
Mitsubishi Xantar® 25 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity Number |
Mitsubishi Xantar® 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity Number |
Mitsubishi Xantar® F 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity Number |
Mitsubishi Xantar® FC 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity Number |
Mitsubishi Xantar® FC 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity Number |
Mitsubishi Xantar® F 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity number |
BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity number |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Viscosity Test | 63 cm³/g | 63 cm³/g | Viscosity number |
BASF Ultrason S 2010 PSU Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Viscosity Test | 63 - 65 cm³/g | 63 - 65 cm³/g | Ubbelhode |
Iran Petrochemical (PCC) TG 645 Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chipsInformation provided by Iran Petrochemical Commercial Co. |