Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 150 cm³/g @Temperature 30.0 °C |
150 cm³/g @Temperature 86.0 °F |
Inherent Viscosity in DMF Solution |
Kureha KF Polymer 1550 High Viscosity PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F4MW4 Nylon 6, 40% Glass Fiber and Mineral Reinforced SAXAMID 126F4MW4 is a 40% glass fibers/ mineral reinforced polyamide 6 injection-molding-grade. It has dimensional stability and high strength.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F6 Nylon 6, 30% Glass Fiber SAXAMID 126F6 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Other properties are .. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F6T3 Nylon 6, 30% Glass Fiber and PTFE SAXAMID 126F6T3 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers and 15% PTFE. Because of its high strength and stiffness this grade is often used for stressed parts requiri.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F4 Nylon 6, 20% Glass Fiber SAXAMID 126F4 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F7 Nylon 6, 35% Glass Fiber SAXAMID 126F7 is a polyamide 6 injection-molding-grade reinforced with 35% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Additional properties.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126H Nylon 6, Injection Molding Grade SAXAMID 126H is a general purpose polyamide 6 injection-molding-grade. Benefits are short cycle times and good release properties. Additionally it has a higher content of heat stabilizer which is p.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 136F4Q32 Nylon 6, 20% Glass Fiber SAXAMID 136F4Q32 is a high impact-modified polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 136Q32 Nylon 6, Injection Molding Grade SAXAMID 136Q32 is a high impact-modified polyamide 6 injection-molding-grade.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F10 Nylon 6.6, 50% Glass Fiber SAXAMID 226F10 is a polyamide 6.6 injection-molding-grade reinforced with 50% glass fibers. It has high mechanical strength.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F3 Nylon 6.6, 15% Glass Fiber SAXAMID 226F3 is a polyamide 6.6 injection-molding-grade reinforced with 15% glass fibers. This grade is suitable for applications requiring high strength and very good flow properties during proces.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126 Nylon 6, Injection Molding Grade SAXAMID 126 is a general purpose polyamide 6 injection-molding-grade. Benefits are short cycle times and good release properties.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F2K4 Nylon 6, Glass Fiber/Bead Filled SAXAMID 126F2K4 is a 10% glass fibers and 20% glass beads filled polyamide 6 injection-molding-grade.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity Number |
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performan.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® RS LC3060 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Medium Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3060 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewable sourced ingredi.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | 0.5% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ 27 Nylon 6 A bright polyamide 6 grade of low viscosity suited for the production of carpet yarns.Information provided by ATT Polymers™ |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | 0.5% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ 27C Nylon 6 A bright polyamide 6 grade of low viscosity suited for the production of compounds.Information provided by ATT Polymers™ |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | 0.5% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ 27D Nylon 6 A bright polyamide 6 grade of low viscosity suited for the production of compounds.Information provided by ATT Polymers™ |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number |
BASF Ultramid® A27 E 01 PA66 (Conditioned) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number |
BASF Ultramid® A27 E 01 PA66 (Dry) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® B3K PA6 (Dry) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® C3U PA66/6 (Dry) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties... |