Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 1.20 - 2.50 mm | 0.0472 - 0.0984 in | |
SABIC EPS 760FF Expandable Polystyrene Product Description: Fire retardant expanded Polystyrene EPS 760FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce.. |
|||
Bead Size | 1.20 - 2.50 mm | 0.0472 - 0.0984 in | |
SABIC EPS 763 Expandable Polystyrene Product Description: Standard expanded Polystyrene EPS 763 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS.. |
|||
Bead Size | 1.80 - 2.50 mm | 0.0709 - 0.0984 in | |
Iran Petrochemical (PCC) TPC - 121 HS Expandable Polystyrene TPC - 121 HSApplication: low density blocksInformation provided by Iran Petrochemical Commercial Co. |
|||
Bead Size | 1.25 - 2.50 mm | 0.0492 - 0.0984 in | |
IRPC Polimaxx Pentfoam 193L Expandable Polystyrene General: Pentfoam 139L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application.. |
|||
Bead Size | 1.25 - 2.50 mm | 0.0492 - 0.0984 in | |
IRPC Polimaxx Pentfoam 241F Expandable Polystyrene General: Pentfoam 241F is a regular grade expandable polystyrene containing pentane as blowing agentApplications: Pentfoam 241F is particularly well suited for the manufacture of eps insulation boar.. |
|||
Bead Size | 1.40 - 2.50 mm | 0.0551 - 0.0984 in | |
BASF Neopor® 2200 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |