Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.600 - 1.00 mm | 0.0236 - 0.0394 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 150R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
NOVA Chemicals Dytherm® 150R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.600 - 1.00 mm | 0.0236 - 0.0394 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 250R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
NOVA Chemicals Dytherm® 250R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.600 - 1.00 mm | 0.0236 - 0.0394 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 350R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
NOVA Chemicals Dytherm® 350R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
Ineos Nova Styrocell® M544C Expandable Polystyrene A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell is.. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
Ineos Nova T523C Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for medium density foam.Applications: This grade is used mainly .. |
|||
Bead Size | 0.500 - 1.00 mm | 0.0197 - 0.0394 in | > 95% in this range per Berre Laboratory Analytical Methods 0492 |
Ineos Nova T543B Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for medium density foam.Applications: This grade is used mainly .. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
Ineos Nova T543B Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for medium density foam.Applications: This grade is used mainly .. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
Iran Petrochemical (PCC) TPC - 323 FC Expandable Polystyrene TPC - 323 FCApplications: faster cycling shape molding with wall thickness >10mm, medium to high density blocksInformation provided by Iran Petrochemical Commercial Co. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Bead Size | 0.600 - 1.00 mm | 0.0236 - 0.0394 in | |
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be.. |
|||
Bead Size | 0.600 - 1.00 mm | 0.0236 - 0.0394 in | |
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S332 which will lead the industry in.. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
BASF Styropor® F 315-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati.. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
BASF Styropor® F 395 -N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
BASF Peripor® 300 Expandable Polystyrene Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low .. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
Iran Petrochemical (PCC) TPC - 321 HS Expandable Polystyrene TPC - 321 HSApplications: shape molding with wall thickness > 10 mm, medium to high density blocksInformation provided by Iran Petrochemical Commercial Co. |
|||
Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
Iran Petrochemical (PCC) TPC - 326 WP Expandable Polystyrene TPC - 326 WPApplications: low water absorption, longer cycling shape molding with wall thickness >10 mmInformation provided by Iran Petrochemical Commercial Co. |