Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.360 - 0.850 mm | 0.0142 - 0.0335 in | Carrington Laboratory Analytical Methods 2155 |
Ineos Nova Styrocell® M742C Expandable Polystyrene A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M742C is used ma.. |
|||
Bead Size | 0.350 - 0.850 mm | 0.0138 - 0.0335 in | >97%, 2% max <0.35 |
BASF Styropor® BF 422 EPS Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv.. |
|||
Bead Size | 0.420 - 0.850 mm | 0.0165 - 0.0335 in | >97%, 2% max <0.425 |
BASF Styropor® BFL 422 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |