Physical Properties Metric English Comments
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
NOVA Chemicals Dytherm® 170F Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 170R Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
NOVA Chemicals Dytherm® 170R Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 270R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
NOVA Chemicals Dytherm® 270R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 370R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
NOVA Chemicals Dytherm® 370R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
Ineos Nova Styrocell® M742C Expandable Polystyrene
A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M742C is used ma..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
Ineos Nova T733B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used after expansion for cellular bricks.Applications: This grade is..
Bead Size 0.500 - 0.700 mm
0.0197 - 0.0276 in
Iran Petrochemical (PCC) TPC - 422 FC Expandable Polystyrene
TPC - 422 FCApplications: shape molding of 6-10mm wall thicknessInformation provided by Iran Petrochemical Commercial Co.
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionThe unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
BASF Styropor® F 415-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foamsApplications: Visible cover pa..
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
BASF Styropor® P 570 Expandable Polystyrene Additive
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: For the production of expanded particles as a filling material ..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
BASF Styropor® F 495-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
BASF Styropor® P 426 Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts.Information pr..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Styrocell® D733A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for contour molding.Applications: This grade is used for dry mol..
Bead Size 0.500 - 0.700 mm
0.0197 - 0.0276 in
NOVA Chemicals Styrocell® D733A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for contour molding.Applications: This grade is used for dry mol..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
BASF Styropor® P 426 C Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts with very shor..
Bead Size 0.500 - 0.700 mm
0.0197 - 0.0276 in
Iran Petrochemical (PCC) TPC - 426 WP Expandable Polystyrene
TPC - 426 WPApplications: very low water absorption, cycling shape molding of 6-10 mm wall thicknessInformation provided by Iran Petrochemical Commercial Co.