Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 1.20 - 2.50 mm | 0.0472 - 0.0984 in | |
SABIC EPS 760FF Expandable Polystyrene Product Description: Fire retardant expanded Polystyrene EPS 760FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce.. |
|||
Bead Size | 1.20 - 2.50 mm | 0.0472 - 0.0984 in | |
SABIC EPS 763 Expandable Polystyrene Product Description: Standard expanded Polystyrene EPS 763 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS.. |
|||
Bead Size | 1.20 - 1.50 mm | 0.0472 - 0.0591 in | |
BASF Neopor® P 5200 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of silver-gray foams having a considerably higher ther.. |