Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.200 - 0.800 mm | 0.00787 - 0.0315 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 170F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Bead Size | 0.200 - 0.400 mm | 0.00787 - 0.0157 in | |
NOVA Chemicals Styrocell® B933A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the .. |
|||
Bead Size | 0.200 - 0.400 mm | 0.00787 - 0.0157 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Styrocell® B933A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the .. |
|||
Bead Size | 0.200 - 0.400 mm | 0.00787 - 0.0157 in | |
BASF Styropor® P 656 Expandable Polystyrene Additive Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: Filling material for lightweight plasters.Information provided .. |
|||
Bead Size | 0.200 - 0.350 mm | 0.00787 - 0.0138 in | |
NOVA Chemicals Styrocell® D933A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic.. |
|||
Bead Size | 0.200 - 0.400 mm | 0.00787 - 0.0157 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Styrocell® D933A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic.. |