Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.900 - 1.40 mm | 0.0354 - 0.0551 in | |
SABIC EPS 650FF Expandable Polystyrene Product Description: Fire retardant expanded Polystyrene EPS 650FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce.. |
|||
Bead Size | 0.900 - 1.40 mm | 0.0354 - 0.0551 in | |
SABIC EPS 652 Expandable Polystyrene Product Description: Standard expanded Polystyrene EPS 652 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS.. |
|||
Bead Size | 1.00 - 1.40 mm | 0.0394 - 0.0551 in | |
Ineos Nova Styrocell® M442C Expandable Polystyrene A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M4.. |
|||
Bead Size | 1.00 - 1.40 mm | 0.0394 - 0.0551 in | |
Ineos Nova T443C Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us.. |
|||
Bead Size | 0.800 - 1.40 mm | 0.0315 - 0.0551 in | |
BASF Neopor® 2300 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Bead Size | 1.22 - 1.40 mm | 0.0480 - 0.0551 in | |
BASF Styropor® KF 162M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 12-30 kg/m3 and fire characteristics in conformity with.. |
|||
Bead Size | 0.700 - 1.40 mm | 0.0276 - 0.0551 in | > 95% in this range per Berre Laboratory Analytical Methods 0492 |
Ineos Nova W441A Expandable Polystyrene A regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for high density foam applications.Applications: This grade is sued mainly for.. |