Polymer Property : Bead Size = 1.70 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 1.70 - 3.15 mm
0.0669 - 0.124 in
> 95% in this range per Berre Laboratory Analytical Methods 0492
Ineos Nova T163B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for very low density foam.Applications: This grade is used mainl..
Bead Size 1.70 - 3.20 mm
0.0669 - 0.126 in
Ineos Nova T163B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for very low density foam.Applications: This grade is used mainl..
Bead Size 1.70 mm
0.0669 in
20.6 wt%
Zircar Ceramics IB-100A Alumina Bubble
Thin wall aluminum oxide ceramic spheres offered in 2 standard bubble sizes. These low density sintered ceramic bodies are useful in a range of refractory applications with temperatures to 2000°C (..
Bead Size 1.70 mm
0.0669 in
13.3 wt%
Zircar Ceramics IB-100B Alumina Bubble
Thin wall aluminum oxide ceramic spheres offered in 2 standard bubble sizes. These low density sintered ceramic bodies are useful in a range of refractory applications with temperatures to 2000°C (..