Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 9.1 g/10 min @Load 21.6 kg, Temperature 190 °C |
9.1 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Sterigenics Raprex® R-200 Branched High Density Polyethylene Applications: Injection Molding and ExtrusionRAPREX® R-200 is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its .. |