Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 6.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
High Load Melt Index | 6.0 - 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.0 - 10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 8250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
High Load Melt Index | 6.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorPEX™ HE2550 High Density Polyethylene Powder for Crosslinked Pipes BorPEX HE2550 is a high molecular weight, high density polyethylene powder for crosslinkable pipes, specially designed for peroxide crosslinking. It is a special polymer, stabilized for transportin.. |
|||
High Load Melt Index | 6.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorPEX™ HE2556 Black High Density Polyethylene Powder for Crosslinked Pipes BorPEX HE2556 is a black, high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for peroxide crosslinking. Well dispersed carbon black give outstand.. |
|||
High Load Melt Index | 6.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2557 is a yellow, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long term stability and UV resistance is .. |
|||
High Load Melt Index | 6.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorPEX™ HE2558 Blue High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2558 is a blue, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long stability and UV resistance is ensured.. |
|||
High Load Melt Index | 6.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB1460 HDPE for Film Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utiliz.. |
|||
High Load Melt Index | 6.0 g/10 min @Load 21.6 kg, Temperature 260 °C |
6.0 g/10 min @Load 47.6 lb, Temperature 500 °F |
|
Ashley Polymers Ashlene® PC/ABS Alloy 306 General purpose with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |