Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 50 g/10 min @Load 21.6 kg |
50 g/10 min @Load 47.6 lb |
ISO 1133 |
Total Finathene® 6006 HDPE, blow molding, pipe
(discontinued **) Finathene® 6006 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Polymerization is conducted in the absence of any other comonomer. Finathene® 6006 h.. |
|||
High Load Melt Index | 50 g/10 min @Load 21.6 kg, Temperature 190 °C |
50 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE2280 BLACK MASTERBATCH BLACK PE2280 is an economy , high tinting strength black masterbatch based on LDPE containing high opacity carbon black. It is designed for use in jet black, high gloss injection molding items, shee.. |
|||
High Load Melt Index | 50 g/10 min @Load 21.6 kg, Temperature 190 °C |
50 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE-B1301 BLACK MASTERBATCH BLACK PE-B1301 is a black low density polyethylene based masterbatch containing pure high opacity carbon black. It is designed for use in high jet black film with excellent surface performance, such.. |
|||
High Load Melt Index | 50 g/10 min @Load 21.6 kg, Temperature 190 °C |
50 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE401A GREEN MASTERBATCH GREEN PE 401A is a green LDPE based masterbatch containing 16% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Green 7.Method of Usage: GREEN PE 401A is designed f.. |