Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 5.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Novapol® HB-W555-EC HDPE Blow Molding Resin HB-W555-EC complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolo.. |
|||
High Load Melt Index | 5.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® C579 High density polyethylene
(discontinued **) Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceApplications: multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containersInformation pro.. |
|||
High Load Melt Index | 5.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Formosa Plastics Formolene® HL4506 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight Hexene CopolymerApplications: Multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containers (IBC)Formolene HL4506 is intended for large part blow molding appl.. |
|||
High Load Melt Index | 5.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Formosa Plastics Formolene® HL5505 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight CopolymerApplications: 55 gallon drums (even those with demanding built-in handling rings), industrial tanksFormolene HL5505 is intended for large part blow molding appli.. |
|||
High Load Melt Index | 5.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE900 BLACK MASTERBATCH BLACK PE900 is an economy black LDPE based masterbatch containing high opacity carbon black. This product is designed for Injection Molding items, extruded tubings and sheets for general purpose. It.. |
|||
High Load Melt Index | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238 |
Ineos K54-05 HDPE K54-05 is a high molecular weight, high density polyethylene copolymer developed for large-part blow molding (drum market) where the finished product demands outstanding physical performance. This m.. |
|||
High Load Melt Index | 5.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ GERS-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ GERS-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |