Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 34 dynes/cm | 34 dynes/cm | 25°C |
LyondellBasell PMP Propylene glycol methyl ether propionate Information provided by Lyondell. |
|||
Surface Tension | 34 - 36 dynes/cm | 34 - 36 dynes/cm | 2nd surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Surface Tension | 34 dynes/cm | 34 dynes/cm | at CMC |
Solvay IGEPAL® CO 710 Surfactant Chemical Name: NONYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHEDCAS: 68412-54-4 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CO-710 is an excellent prima.. |
|||
Surface Tension | 34 dynes/cm | 34 dynes/cm | |
BASF Ecoflex® 1200 F Blend Biodegradable Polyester Description: A flexible plastic designed for film extrusion and extrusion coating. Ecoflex® F Blend 1200 comes closer than any other biodegradable plastic to the processing properties of LDPE and L.. |
|||
Surface Tension | 34 dynes/cm | 34 dynes/cm | |
Solvay RHODASURF® TR/15-40 Surfactant Identification: WATER SOLUTION OF ETHOXYLATED TRIDECYL ALCOHOLCAS: 9043 – 30 – 5 ; 7732 – 18 – 5Solubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Available in:.. |
|||
Surface Tension | 34 dynes/cm | 34 dynes/cm | |
Solvay RHODOCLEAN® ASP Surfactant Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Applications: Surfactant for metal working app.. |