Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Surface Tension = 35 dynes/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Surface Tension 35 - 45 dynes/cm
35 - 45 dynes/cm
Method L-005/L-040; ASTM D1417
Nitriflex Nitrilatex NTL-350 Styrene Butadiene Latex
NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesive..
Surface Tension 35 - 50 dynes/cm
35 - 50 dynes/cm
Ring Type; LSY-QB-ID005
LG Chemical Lutex 703 SBR Latex
Description: Binding Force, Ink set off, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Pre-Rod, Blade Coater, Adhesive coated paper and Carpet back-coating ..
Surface Tension 35 - 45 dynes/cm
35 - 45 dynes/cm
Ring Type; LSY-QB-ID005
LG Chemical Lutex 760 SBR Latex
Description: Binding Force, Print gloss, High Shear Rheology, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Top-Film, Blade Coater, Adhesive coated paper an..
Surface Tension 35 - 50 dynes/cm
35 - 50 dynes/cm
Ring Type; LSY-QB-ID005
LG Chemical Lutex M710 SBR Latex
Description: High Binding Force (MSP), Ink set off, Print Mottle, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Top-Film Coater, Adhesive coated paper and Carpet back-coating adhesive..
Surface Tension 35 dynes/cm
35 dynes/cm
Ring Method
Asahi Glass Fluon® AD1 PTFE Aqueous Dispersion
Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc...
Surface Tension 35 dynes/cm
35 dynes/cm
30 ppm
3M FC-1100 Acid Mist Suppressant
3M™ Acid Mist Suppressant FC-1100 is a fluorochemical additive that provides outstanding sulfuric acid mist suppression in the copper electrowinning tankhouse without the formation of a stable foam..
Surface Tension 35 dynes/cm
35 dynes/cm
Ring Method
Asahi Glass Fluon® AD936 PTFE Aqueous Dispersion
Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc...