Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 40 Mesh | 40 Mesh | Traces; PVCH/QCD/3514 |
Reliance Industries 57-01 Polyvinyl Chloride Information provided by Reliance IndustriesApplications: Rigid injection. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | Traces; PVCH/QCD/3514 |
Reliance Industries 60-11 Polyvinyl Chloride Information provided by Reliance IndustriesApplications:Recommended:Rigid extrusionRigid injectionRigid calenderingCan be used:Blow molding |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | Traces; PVCH/QCD/3514 |
Reliance Industries 67-11 Polyvinyl Chloride Information provided by Reliance IndustriesApplications: Recommended:Flexible extrusionFlexible injectionFlexible calenderingCan be used:Rigid injectionRigid extrusion |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | Traces; PVCH/QCD/3514 |
Reliance Industries 57-11 Polyvinyl Chloride Information provided by Reliance IndustriesApplications: Rigid injectionRigid extrusionRigid calenderingblow molding |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 20.2% retained |
Imerys G-20 HP Feldspar G-20 HP Feldspar is a high potassium aluminium silicate ground to 200 mesh for ceramic applications. G-20HP offers high potassium content and low iron oxide per unit of alumina.Information provided .. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 0% retained |
Imerys Minsilsparâ„¢ Feldspar Minsilspar is a 170 mesh feldspathic sand (sandspar) used primarily in the Sanitaryware industry.Information provided by Imerys |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 11.3% retained |
Imerys Minsparâ„¢ 1 Feldspar Minspar 1 is a minus 30 mesh Feldspar product used in the glass container and ceramic tile markets.Information provided by Imerys |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 0% retained |
Imerys Minsparâ„¢ 200 Feldspar Minspar 200 is 200 mesh flotation grade soda Feldspar used in the ceramic whiteware industry for sanitaryware, dinnerware, floor and wall tile, artware and glazes.Information provided by Imerys |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | Opening 1700µm; ASTM E11 |
Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and th.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% min; ASTM D1921 |
Westlake 1195 PVC Westlake PVC 1195 resin is a low molecular weight resin designed for rigid injection molding, calendering, sheet extrusion, and blow molding.Information provided by Westlake Chemical Corporation |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% min; ASTM D1921 |
Westlake 1230P PVC Westlake PVC 1230P resin is a general purpose, medium molecular weight homopolymer designed primarily for the extrusion of rigid PVC products.Information provided by Westlake Chemical Corporation |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% min; ASTM D1921 |
Westlake 1230S PVC Westlake PVC 1230S resin is a medium molecular weight homopolymer designed primarily for the extrusion of rigid products.Information provided by Westlake Chemical Corporation |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; ASTM D1921B |
Formosa Plastics Formolon® 113 PVC PVC Copolymer Suspension Resin F-113 has been developed primarily to meet the processing requirements of the vinyl composition tile (VCT) manufacturers. In addition to vinyl floor tile industry, F-1.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 100% thru; ASTM D1921B |
Formosa Plastics Formolon® 260 PVC PVC Homopolymer Blending Resin F-260 is a fine particle size PVC homopolymer plastisol blending resin. It combines excellent fusion characteristics, low plastisol viscosities as well as lot to lot u.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 100% thru; ASTM D1921B |
Formosa Plastics Formolon® 265 PVC PVC Copolymer Blending Resin F-265 is a fine particle size polyvinyl chloride vinyl acetate copolymer plastisol blending resin. The product has been designed for use in application where rapid gelat.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 608 PVC PVC Homopolymer General Purpose Grade Resin F608 is a low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels and exc.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 614 PVC Homopolymer - General Purpose Grade Resin F614 is a medium-low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels an.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 622E PVC Rigid Extrusion Resin F622E is a medium-low molecular weight PVC designed primarily for rigid extrusion applications. This product has excellent dry flow characteristics, making it desirable for dry.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 622R PVC Homopolymer General Purpose Grade Resin F622R is a medium-low molecular weight PVC homopolymer of interest in both rigid and flexible applications and has established a deserved reputation for low .. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 676 PVC Homopolymer General Purpose Grade Resin F676 is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered .. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 680 PVC Homopolymer General Purpose Grade Resin F680 is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, thi.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 690 PVC Homopolymer General Purpose Grade Resin F690 is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, thi.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 90-100%; US std sieve |
Zeon Chemicals Zealloy® 1422 Modifier for Thermoplastics Zealloy 1422 is a copolymer of butadiene and acrylonitrile of medium oil resistance. It is furnished as a finely-divided powder. Sufficient antioxidant is added during manufacture for normal storage.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 622F PVC Homopolymer Film Grade Resin F622F is a medium molecular weight PVC homopolymer suitable for both rigid extrusion applications and it is suitable for many flexible applications. This product has goo.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 680H PVC Homopolymer General Purpose Grade Resin F680H is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, th.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 99.9% thru; Malvern |
Formosa Plastics Formolon® 685 PVC Homopolymer General Purpose Grade Resin F685 is especially suited for processing from powder blends due to its ability to absorb plasticizers regardless of molecular weight. In addition, this produc.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 90-100%; US std sieve |
Zeon Chemicals Nipol® 1411 Nitrile Powder and Crumb Elastomer Nipol 1411 is a copolymer of butadiene and high acrylonitrile, furnished as a very fine powder. This material contains sufficient antioxidant for normal storage condition.very fine crosslinked powde.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | 91.0% passing, dry |
CIMBAR Suspengel™ 16 High Purity Bentonite, Industrial Grade Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co.. |
|||
Particle Mesh Size | 40 Mesh | 40 Mesh | Traces; PVCH/QCD/3514 |
Reliance Industries 70-21 Polyvinyl Chloride Information provided by Reliance IndustriesApplications:Can be used:Flexible extrusionFlexible injectionFlexible calendering |
|||
Particle Mesh Size | 40 - 50 Mesh | 40 - 50 Mesh | US Sieve |
Potters Industries A-Series P-0170 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |