Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 80 - 120 Mesh | 80 - 120 Mesh | US Sieve |
Potters Industries A-Series P-0070 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Mesh Size | >= 80 Mesh | >= 80 Mesh | 80%; ASTM E11-87 |
Minelco FireCarb TEG-315 Expandable Graphite High quality crystalline flake graphite that has a medium to high source of carbon, typically 80 – 99%Expandable graphite belongs to a group of products called "intumescents." The primary prope.. |
|||
Particle Mesh Size | 80 Mesh | 80 Mesh | 55-90% |
H.C. Starck Amperweld® 1701.39 K1 Chromium Carbide RIII HS Number: 284990 |
|||
Particle Mesh Size | 80 Mesh | 80 Mesh | 0-10 % |
Lehigh Technologies 80 Mesh Ground Reclaimed Whole Tire Rubber A free flowing black powder produced from vulcanized rubber materialInformation provided by Lehigh Technologies, LLC. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem 475-860N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem AB835EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem AB835EM-1 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed unconventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, completel.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem AB845EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem AB-860LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem AB870EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem AB870LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem DIOSHY® GP-935-UB2 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem DIOSHY® MP-960NC TPE Compound This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem FP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem GP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem GP-9401 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem GP-945 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem GP-950 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem GP-980 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem LP-855 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem LP-880 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem MP-850 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem MP-930HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem MP-950NC TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Particle Mesh Size | 80 - 150 Mesh | 80 - 150 Mesh | |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Particle Mesh Size | 80 Mesh | 80 Mesh | D4570-89 |
Zeon Chemicals Zisnet® F-PT Polyepichlorohydrin and Polyacrylate Curing Agent Zisnet® F-PT is a unique curative that provides a safe curing system alternative to red lead/ethylene thiorea. Curing characteristics of Zisnet® F-PT can be developed to be the same as the red lea.. |