Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 230 Mesh | 230 Mesh | 5%; Geon® 812 |
PolyOne Geon™ 140 Series 140X466 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shippin.. |
|||
Particle Mesh Size | 230 Mesh | 230 Mesh | 5%; Geon® 812 |
PolyOne Geon™ 140 Series 140X484 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shippin.. |
|||
Particle Mesh Size | 230 Mesh | 230 Mesh | 5%; Geon® 812 |
PolyOne Geon™ 140 Series 140X497 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shippin.. |
|||
Particle Mesh Size | 230 Mesh | 230 Mesh | Minimum of 70% |
H.C. Starck Amperweld® 1701.39 K2 Chromium Carbide RIII HS Number: 284990 |
|||
Particle Mesh Size | 230 Mesh | 230 Mesh | Minimum of 85% |
H.C. Starck Amperweld® 1701.39 K3 Chromium Carbide RIII HS Number: 284990 |
|||
Particle Mesh Size | 230 Mesh | 230 Mesh | screening fraction max 0.5%; Sieve Analysis per ASTM B214 |
H.C. Starck MoMP 3.5 - 4.5 micron Molybdenum Metal Powder, Mo (99.95%) Description of Product: Grey metal powder. Sieved.Typical Applications: The production of pressed and sintered Mo or Mo alloy parts. Also used to produce blended alloy powders.Information provid.. |
|||
Particle Mesh Size | 230 Mesh | 230 Mesh | screening fraction max 0.5%; Sieve Analysis per ASTM B214 |
H.C. Starck MoMP 4.5 - 5.5 micron Molybdenum Metal Powder, Mo (99.95%) Description of Product: Grey metal powder. Sieved.Typical Applications: The production of pressed and sintered Mo or Mo alloy parts. Also used to produce blended alloy powders.Information provid.. |
|||
Particle Mesh Size | 230 Mesh | 230 Mesh | Opening 1700µm; ASTM E11 |
Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and th.. |