One Hour Half Life Temperature 141 °C
286 °F
Akzo Nobel Trigonox® B-C30 Polymerization Initiator
Initiator for the (co)polymerization of ethylene.Chemical Description: Di-tert-butyl peroxide, 30% solution in odorless mineral spiritsCAS Number: 110-05-4Acronym: DTBP; Tx BInformation provided by ..
One Hour Half Life Temperature 141 °C
286 °F
Akzo Nobel Trigonox® B-C50 Polymerization Initiator
Initiator for the (co)polymerization of ethylene.Chemical Description: Di-tert-butyl peroxide, 50% solution in odorless mineral spirits CAS Number: 110-05-4Acronym: DTBP; Tx BInformation provided by..
One Hour Half Life Temperature 141 °C
286 °F
Akzo Nobel Trigonox® B Polymerization Initiator
Initiator for the (co)polymerization of ethylene, styrene, acrylates and methacrylates. Trigonox B is a monofunctional peroxide which is used for the crosslinking of polyolefins as well as natural r..