Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3000 - 4000 cP | 3000 - 4000 cP | DOP 60phr, 6RPM; ASTM D1824-90 |
LG Chemical LP170G PVC General Description: LP170G, homopolymer made from micro- suspension polymerization, is a low viscosity PVC resin with an good deaeration and stable viscosity at high temperature. Products made from.. |
|||
Brookfield Viscosity | 2000 - 4000 cP | 2000 - 4000 cP | DOP 60phr, 6RPM; ASTM D1824-90 |
LG Chemical LP170L PVC General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for .. |
|||
Brookfield Viscosity | 1000 - 4000 cP | 1000 - 4000 cP | Spindle # 3, rpm 30 |
Michelman® Michem® Prime 4983-40R Ethylene acrylic acid dispersion Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 498340R is a high solids, more economical version of Michem® Prime 4983R. Like Michem® Prime 4983R, this product provides o.. |
|||
Brookfield Viscosity | 1500 - 4000 cP | 1500 - 4000 cP | RVF #4 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Brookfield Viscosity | 2500 - 4000 cP | 2500 - 4000 cP | RVT #3 sp @ 20 rpm |
3M Scotch-Weld™ TL43 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Brookfield Viscosity | 100 - 4000 cP | 100 - 4000 cP | RVF #4 sp @ 20 rpm @ 27°C |
3M Scotch-Weld™ 4550 Industrial Adhesive Features: It is a sprayable, synthetic elastomer based adhesive for bonding many lightweight materials such as felt, cork, cardboard, and paper to metal and other substratesIdeal for palletizing “a.. |
|||
Brookfield Viscosity | 2000 - 4000 cP | 2000 - 4000 cP | RVF #3 sp @ 10 rpm |
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions a.. |