Polymer Property : Brookfield Viscosity = 3.0 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 1.0 - 3.0 cP

@Temperature 20.0 °C
1.0 - 3.0 cP

@Temperature 68.0 °F
Brookfield RVT spindle 2.2 RPM
C.O.I.M. FILCO® 354 N Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing
Description: Unsaturated Bisphenolic Polyester Polymer for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in ..