Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 310 - 390 cP @Temperature 30.0 °C |
310 - 390 cP @Temperature 86.0 °F |
|
Lubrizol Telene 1650 A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |