Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 27000 cP | 27000 cP | Acecelerator, DV-II, #7 sp, 20 rpm |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Brookfield Viscosity | 27000 cP | 27000 cP | Acecelerator, DV-II, #7 sp, 20 rpm |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |