Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2100 - 2500 cP @Temperature 20.0 °C |
2100 - 2500 cP @Temperature 68.0 °F |
Brookfield RVF sp. 4, 20 rpm solution at 15% in MEK; MQSA N° 40A |
Lubrizol Advanced Materials Pearlstick® 49-46/23 Linear Thermoplastic Polyurethane Elastomer
(discontinued ** Pearlstick 49-46/23 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low thermoplasticity level, available as pellets.Solubility: Pearlstick 49-46/23 is solu.. |
|||
Brookfield Viscosity | <= 2100 cP | <= 2100 cP | Spindle # 4, rpm 60 |
Michelman® Michem® Dispersion 471 Solvent dispersion of carnauba wax Description: Solvent dispersion of carnauba waxUsage: Michem® Dispersion 471 provides slip and abrasion resistance. This product has proven very effective for slip and abrasion resistance when us.. |
|||
Brookfield Viscosity | 2100 cP | 2100 cP | RVT |
Gromax EP-5016M Unplasticized Vinyl Acetate homopolymer Product Description: EP-5016M is a water redispersible vinyl acetate homopolymer powder that is readily dispersible in water and forms stable emulsion. This redispersible powder is especially recomm.. |
|||
Brookfield Viscosity | 2100 - 2900 cP | 2100 - 2900 cP | Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® D40-70/25 Linear Thermoplastic Polyurethane Pearlstick D40-70/25 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. .. |
|||
Brookfield Viscosity | 2100 cP @Temperature 23.9 °C |
2100 cP @Temperature 75.0 °F |
Mixed |
BCC Products BC 5009 General Purpose Epoxy System BC5009 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC5009 is a clear-amber epoxy adhesive especially formulated for the bonding of wood and u.. |