Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 17000 cP @Temperature -40.0 °C |
17000 cP @Temperature -40.0 °F |
|
ChevronTexaco Synthetic All-Weather THF FeaturesChevron All-Weather THF is a truly unique, high quality, multifunctional fluid, specially formulated for use in transmissions, final drives, wet brakes, and hydraulic systems of tractors and.. |
|||
Brookfield Viscosity | 17000 cP @Temperature -40.0 °C |
17000 cP @Temperature -40.0 °F |
|
ChevronTexaco TDH® SS Oil Texaco TDH Oil SS delivers value through:Reduced operational costs — Excellent performance in a wide range of ambient and operating temperatures provides year-round improved low temperature hydraul.. |
|||
Brookfield Viscosity | 17000 cP @Temperature -35.0 °C |
17000 cP @Temperature -31.0 °F |
|
ChevronTexaco TDH® W Oil Texaco TDH oils deliver value through:Lower operating costs — By delivering or exceeding the performance of fluids supplied by equipment manufacturers, helps in avoiding the cost of generally more .. |
|||
Brookfield Viscosity | 17000 cP @Temperature -40.0 °C |
17000 cP @Temperature -40.0 °F |
|
ChevronTexaco THF W FeaturesChevron THF W is a high quality, multifunctional fluid, specially formulated for low temperature use in transmissions, final drives, wet brakes, and hydraulic systems of tractors and other e.. |
|||
Brookfield Viscosity | 17000 cP @Temperature 177 °C |
17000 cP @Temperature 350 °F |
ASTM D1084 |
Dow AFFINITY™ GA 1950 Polyolefin Plastomer (POP) AFFINITY™ GA 1950 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and.. |
|||
Brookfield Viscosity | 17000 cP @Temperature -40.0 °C |
17000 cP @Temperature -40.0 °F |
|
ChevronTexaco DEXRON®-III/MERCON® Automatic Transmission Fluid General DescriptionDEXRON® is a specification for General Motors vehicles, but many foreign manufactures specify a DEXRON approved ATF as well. DEXRON-III can be used in transmissions that call for.. |
|||
Brookfield Viscosity | 17000 cP | 17000 cP | Base, DV-II, #7 sp, 20 rpm |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Brookfield Viscosity | 17000 - 30000 cP | 17000 - 30000 cP | Base, DV-II, #7 sp, 20 rpm |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Brookfield Viscosity | 17000 cP @Temperature -40.0 °C |
17000 cP @Temperature -40.0 °F |
|
ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid Havoline Automatic Transmission Fluid MERCON/DEXRON-III delivers value through:Protection against the formation of lacquers, sludge, or other harmful deposits.Exceptional stability provided by excel.. |