Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 15000 - 45000 cP | 15000 - 45000 cP | DOP 60phr; ASTM D1824 |
LG Chemical PB1120 PVC General Description: PB1120, homopolymer made by micro-suspension seeded polymerization, is medium-viscosity PVC resin with pseudo plastic flow property. It can be used for foam flooring layer and w.. |
|||
Brookfield Viscosity | 15000 - 23000 cP @Temperature 25.0 °C |
15000 - 23000 cP @Temperature 77.0 °F |
Spindle CP52 @ 10rpm |
Lord Adhesives Thermosetâ„¢ MS-330 Silicone Board Level Encapsulant LORD Thermosetâ„¢ MS-330 encapsulant is a one component silicone specifically designed for use on high-frequency devices including Bluetooth applications. This silicone encapsulant offers excelle.. |
|||
Brookfield Viscosity | 15000 cP @Temperature 25.0 °C |
15000 cP @Temperature 77.0 °F |
|
Loctite® 3525 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 15000 cP @Temperature 163 °C |
15000 cP @Temperature 325 °F |
|
3M Scotch-Weld™ 3794 Hi Tack PSA Bulk only Adhesive Sprayable high tack PSA for bonding plastic, paper, metals, die-cut labelsInformation provided by 3M |
|||
Brookfield Viscosity | 15000 - 30000 cP | 15000 - 30000 cP | Base, DV-II, #7 sp, 20 rpm |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Brookfield Viscosity | 15000 - 55000 cP | 15000 - 55000 cP | Accelerator, RVF #5 sp @ 10 rpm |
3M Scotch-Weld™ DP640 Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl.. |
|||
Brookfield Viscosity | 15000 cP @Temperature 23.9 °C |
15000 cP @Temperature 75.0 °F |
Mixed |
BCC Products BC 7136 Epoxy Casting BC7136 is a gray, low toxicity, aluminum filled, epoxy casting resin. This heat resistant system may be used at room temperature without post-curing. May be cast to a thickness of ¾ inch in non-con.. |
|||
Brookfield Viscosity | 15000 - 40000 cP | 15000 - 40000 cP | Accelerator, RVF #5 sp @ 20 rpm |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Brookfield Viscosity | 15000 - 40000 cP | 15000 - 40000 cP | Accelerator, RVF #5 sp @ 20 rpm |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Brookfield Viscosity | 15000 - 40000 cP | 15000 - 40000 cP | Accelerator, RVF #5 sp @ 20 rpm |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |