Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1100 cP | 1100 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 2430 Styrene - Butadiene Copolymer Europrene Latice® 2430 is an aqueous dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contai.. |
|||
Brookfield Viscosity | 1100 cP | 1100 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1161 B (SIS) Linear Block Copolymer Description: Kraton D1161 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra.. |
|||
Brookfield Viscosity | 1100 cP | 1100 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1191 E (SBS) Radial Block Copolymer Description: Kraton D1191 E is a clear, radial block copolymer based on styrene and butadiene with bound styrene of 33.5% mass. It is supplied from Europe in the physical forms described: Kraton D11.. |
|||
Brookfield Viscosity | 1100 - 1700 cP @Temperature 20.0 °C |
1100 - 1700 cP @Temperature 68.0 °F |
Brookfield RVF sp. 6, 20 rpm solution at 15% in MEK; MQSA N0 40A |
Lubrizol Advanced Materials Pearlstick® 48-60/15 Linear Thermoplastic Polyurethane Elastomer Pearlstick 48-60/15 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low-medium thermoplasticity level, available as pellets.Solubility: Pearlstick 48-60.. |
|||
Brookfield Viscosity | 1100 - 1600 cP | 1100 - 1600 cP | Brookfield RVF sp 4, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® D40-70/14 Linear Thermoplastic Polyurethane Pearlstick D40-70/14 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. .. |
|||
Brookfield Viscosity | 1100 cP @Temperature 25.0 °C |
1100 cP @Temperature 77.0 °F |
|
Loctite® 3051 Light Cure Acrylic Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 1100 cP @Temperature 25.0 °C |
1100 cP @Temperature 77.0 °F |
|
Loctite® 3491 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 1100 cP | 1100 cP | 25% toluene solution; MA 04-3-064 |
Dynasol Calprene® 540 Thermoplastic Rubber SBS Dry Calprene 540 is a 60/40 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure. This product is presented in pellet form and has excellent optical propertie.. |
|||
Brookfield Viscosity | 1100 - 1300 cP @Temperature 25.0 °C |
1100 - 1300 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 110 Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 110: Highly reactive.. |
|||
Brookfield Viscosity | 1100 - 6000 cP | 1100 - 6000 cP | Part B, CP#52 @ 100 rpm |
3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling 3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigg.. |
|||
Brookfield Viscosity | 1100 - 6000 cP | 1100 - 6000 cP | Part B, CP #52 @ 100 rpm |
3M Scotch-Weld™ DP601 Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Brookfield Viscosity | 1100 cP | 1100 cP | 25% toluene solution; MA 04-3-064 |
Dynasol Calprene® 500 Thermoplastic Rubber SBS Dry Calprene 500 is a 70/30 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure. This product is presented in pellet form and has excellent optical propertie.. |