Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 250 - 450 cP | 250 - 450 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Coat 40 Plus Water resistant, gluable coating Description: Water resistant, gluable coatingUsage: Michem® Coat 40 Plus is a water-based coating designed to provide good water resistance to corrugated board while being cold set gluable with m.. |
|||
Brookfield Viscosity | 180 - 450 cP @Temperature 23.0 °C |
180 - 450 cP @Temperature 73.4 °F |
|
Lucite International Series 100 Liquid Acrylic Resin LUCITE® LIQUID ACRYLIC RESINS SERIES 100For the manufacture of solid surface shapesAmbient temperature cureCan be used on batch or continuous in-line mixing equipmentInformation provided by Lucit.. |
|||
Brookfield Viscosity | 150 - 450 cP | 150 - 450 cP | Brookfield RVF sp 2, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 45-90/03 Polycaprolactone based TPU Pearlstick 45-90/03 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a low crystallization.. |
|||
Brookfield Viscosity | 350 - 450 cP @Temperature 25.0 °C |
350 - 450 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 104 L Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 104 L: Same performa.. |
|||
Brookfield Viscosity | 350 - 450 cP @Temperature 25.0 °C |
350 - 450 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 108 A Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 108 A: Resin for van.. |
|||
Brookfield Viscosity | 350 - 450 cP @Temperature 25.0 °C |
350 - 450 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 902 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 902: Flexible resin .. |
|||
Brookfield Viscosity | 200 - 450 cP | 200 - 450 cP | RVF #2 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |