Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 750 - 1250 cP @Temperature 25.0 °C |
750 - 1250 cP @Temperature 77.0 °F |
25% Toluene solution; BAM 922 |
Kraton® D1111 K (SIS) Linear Block Copolymer Description: Kraton D1111 K is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: .. |
|||
Brookfield Viscosity | 150 - 1250 cP | 150 - 1250 cP | RVT Model, Spindle #3 @ 20 rpm |
3M 32661 Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Brookfield Viscosity | 150 - 1250 cP | 150 - 1250 cP | RVT Model, Spindle #3 @ 20 rpm |
3M 32662 Black Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Brookfield Viscosity | 150 - 1250 cP | 150 - 1250 cP | RVT Model, Spindle #3 @ 20 rpm |
3M 32665 Green Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Brookfield Viscosity | 150 - 1250 cP | 150 - 1250 cP | RVT Model, Spindle #3 @ 20 rpm |
3M 32666 Tan Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Brookfield Viscosity | 750 - 1250 cP | 750 - 1250 cP | RVF #2 sp @ 20 rpm @ 27°C |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |
|||
Brookfield Viscosity | 450 - 1250 cP | 450 - 1250 cP | RVF #3 sp @ 20 rpm @ 27°C |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |
|||
Brookfield Viscosity | 150 - 1250 cP | 150 - 1250 cP | RVT Model, Spindle #3 @ 20 rpm |
3M 32663 Medium Grey Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Brookfield Viscosity | 150 - 1250 cP | 150 - 1250 cP | RVT Model, Spindle #3 @ 20 rpm |
3M 32664 Light Gray Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |