Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 90000 - 110000 cP @Temperature 25.0 °C |
90000 - 110000 cP @Temperature 77.0 °F |
RVT, Spindle #7 @ 20rpm |
Lord Adhesives Metech 3270 Silver Conductor This composition is a silver bearing paste designed for screen print application of a fired conductive electrode. It forms a highly adherent bond to many compositions including alumina. The paste ha.. |
|||
Brookfield Viscosity | 90000 cP @Temperature -26.0 °C |
90000 cP @Temperature -14.8 °F |
|
ChevronTexaco Multigear® LS SAE 80W-90 Texaco Multigear LS delivers value through:Reduced inventory costs — One gear lubricant for both conventional and limited slip differentials. Simplified inventory saves money, space, handling time .. |
|||
Brookfield Viscosity | 90000 cP @Temperature -26.0 °C |
90000 cP @Temperature -14.8 °F |
|
ChevronTexaco Supreme LS SAE 80W-90 Supreme LS Gear Lubricant FeaturesChevron Supreme LS Gear Lubricant is a high quality multipurpose gear lubricant.It is formulated with friction modifiers so that it can be used for complete replacement or top-off in limited.. |
|||
Brookfield Viscosity | 90000 - 150000 cP | 90000 - 150000 cP | Base, RVF #6 spindle, 20 rpm @ 27°C |
3M Scotch-Weld™ DP-100NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP-100NS is a two-part adhesives offering fast cure and machinability.Information provided by 3M |