Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 4.43 cP | 4.43 cP | Initial Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ 120 Series 121A Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 121A is high molecular weight resin providing good fused film physical properties. It provides good chemical foamability for producing medium to high density foams. It gives good dispersabili.. |
|||
Brookfield Viscosity | 4.43 cP | 4.43 cP | Initial Viscosity @ 20 rpmGeon® ALTC 22 (with provided formulation); Internal Method |