Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3000 - 8000 cP | 3000 - 8000 cP | DOP 60phr, 6RPM; ASTM D1824-90 |
LG Chemical LP170 PVC General Description: LP170, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170 can be used for sy.. |
|||
Brookfield Viscosity | 3000 - 4000 cP | 3000 - 4000 cP | DOP 60phr, 6RPM; ASTM D1824-90 |
LG Chemical LP170G PVC General Description: LP170G, homopolymer made from micro- suspension polymerization, is a low viscosity PVC resin with an good deaeration and stable viscosity at high temperature. Products made from.. |
|||
Brookfield Viscosity | 3000 cP | 3000 cP | 9924A; ASTM D2196-66; LVT, Spindle #3 @ 12rpm |
Lord Adhesives Aeroglaze® 9924 Wash Primer Aeroglaze® 9924 wash primer was designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.All information provided by .. |
|||
Brookfield Viscosity | 3000 cP | 3000 cP | 9924A; ASTM D2196-66; LVT, Spindle #3 @ 12rpm |
Lord Adhesives Aeroglaze® 9924V Wash Primer Aeroglaze® 9924V wash primer was designed for priming metal surfaces. It is particularly useful for priming non-ferrous substrates such as aluminum and galvanized steel.All information provided b.. |
|||
Brookfield Viscosity | 3000 cP | 3000 cP | ASTM D2196-66; LVT, Spindle #2 @ 30rpm |
Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul.. |
|||
Brookfield Viscosity | 3000 - 22500 cP | 3000 - 22500 cP | Fusor 2001; LVT, Spindle #4 @ 30rpm |
Lord Adhesives Fusor® 2001 / 2002 Urethane Adhesive Fusor® 2001/2002 is a two-part urethane adhesive system used to bond fiberglass reinforced plastics, sheet molded compound, and bulk molded compound to themselves as well as to primed metals.All .. |
|||
Brookfield Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | Measured on 25% mass solution in toluene at 25°C; KM 06 |
Kraton® D1101 B (SBS) Liner Block Copolymer Description: Kraton D1101 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from South America in the physical form(s) identifi.. |
|||
Brookfield Viscosity | 3000 cP @Temperature 23.0 °C |
3000 cP @Temperature 73.4 °F |
20% T.S. in MEK; 20 RPM; RVT Spindle #2 |
Lubrizol Estane® 5712 Thermoplastic Polyurethane Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl.. |
|||
Brookfield Viscosity | 3000 - 5000 cP @Temperature 191 °C |
3000 - 5000 cP @Temperature 375 °F |
|
3M Scotch-Weld™ 6111 Green Bulk only Adhesive Same as 6111 tan but green in colorInformation provided by 3M |
|||
Brookfield Viscosity | 3000 cP | 3000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ EZ250120 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Brookfield Viscosity | 3000 cP | 3000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Brookfield Viscosity | 3000 cP | 3000 cP | Part A; ASTM D2393 |
BCC Products DP-11-88 Urethane Adhesive DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions .. |
|||
Brookfield Viscosity | 3000 - 5000 cP @Temperature 191 °C |
3000 - 5000 cP @Temperature 375 °F |
|
3M Scotch-Weld™ 6111 Tan Bulk only Adhesive Sprayable 100% solventless adhesive for most foams, fabrics, plastics, particle board and thin metalInformation provided by 3M |
|||
Brookfield Viscosity | 3000 cP | 3000 cP | |
BCC Products BC 8675E Polyurethane Elastomer BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f.. |