Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 175 cP | 175 cP | One Hour Viscosity @ 30rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 171 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Brookfield Viscosity | 175 cP | 175 cP | One Hour Viscosity @ 30rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 4195 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Brookfield Viscosity | 175 cP | 175 cP | One Hour Viscosity @ 30 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L120UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L120UF is a high molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for thin.. |
|||
Brookfield Viscosity | 175 cP | 175 cP | One Hour Viscosity @ 30 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L140UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L140UF is an ultra high molecular weight, ultrafine particle size homopolymer dispersion resin. The excellent dispersibility provides good product throughput during the organoso.. |
|||
Brookfield Viscosity | 175 - 800 cP | 175 - 800 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4310 SBR Latex ROVENE® 4310 is a carboxylated styrene-butadiene emulsion that imparts an ultra soft hand when used in backcoating, spray, and “dip and nip†applications. This non-woven, textile, and p.. |
|||
Brookfield Viscosity | 175 - 800 cP | 175 - 800 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 5010 SBR Latex ROVENE® 5010 is a carboxylated styrene-butadiene emulsion that imparts an ultra soft hand when used in backcoating, spray, and “dip and nip†applications. This non-woven, textile, and p.. |
|||
Brookfield Viscosity | 175 - 350 cP | 175 - 350 cP | RVF #2 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 5 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfacesInforma.. |
|||
Brookfield Viscosity | 175 - 350 cP | 175 - 350 cP | RVF #2 sp @ 20 rpm |
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Brookfield Viscosity | 175 - 275 cP | 175 - 275 cP | RVF #2 sp @ 20 rpm @ 27°C |
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt.. |