Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 170000 - 200000 cP @Temperature 25.0 °C |
170000 - 200000 cP @Temperature 77.0 °F |
HBT, Spindle #SC4-14 @ 10rpm |
Lord Adhesives Metech 3571 Silver Conductor Composition This high performance silver conductor is designed for cost sensitive hybrid applications. It employs advanced powders technology with a mix bonded frit system to yield a highly dense fired film tha.. |
|||
Brookfield Viscosity | 170000 - 190000 cP @Temperature 25.0 °C |
170000 - 190000 cP @Temperature 77.0 °F |
HBT, Spindle #SC4-14 @ 10rpm |
Lord Adhesives Metech 7600A Cermet Multilayer Dielectric Composition Dielectric composition 7600A is a glass-ceramic insulative film designed for use in high density multilayer hybrid circuits using either gold or palladium-silver conductors. 7600A fires at 850°C .. |