Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 336 hour | 336 hour | No Failure; Q&T; Test Type - C-Ring; Test Condition - Specimen coupled to carbon steel. 5% NaCl + 0.5% Acetic Acid in H<sub>2</sub>O + 100% H<sub>2</sub>S. |
Crucible Compaction Metals P/M 625 Corrosion Resistant Alloy P/M 625 (chemically, UNS N06625) is produced by the Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The Crucible powder con.. |