Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 8.00 - 1000 hour | 8.00 - 1000 hour | Average value: 373 hour Grade Count:19 |
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m.. |