Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 720 hour | 720 hour | No Failure; Double Age; Test Type - C-Ring; Test Condition - 25% NaCl in H<sub>2</sub>O + a gas mixture of 15% H<sub>2</sub>S, 15% CO<sub>2</sub> and 70% N<sub>2</sub> + lg/l elemental sulfur |
Crucible Compaction Metals P/M 625 Corrosion Resistant Alloy P/M 625 (chemically, UNS N06625) is produced by the Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The Crucible powder con.. |