Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 250 hour | >= 250 hour | ISO 22088 |
Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |
|||
Environmental Stress Crack Resistance | >= 250 hour | >= 250 hour | ASTM D1693 |
NIZHNEKAMSKNEFTEKHIM PE 6751E (516H5) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Environmental Stress Crack Resistance | 250 hour | 250 hour | F50, Igepal, Condition C; ASTM D-1693 |
ExxonMobil Escorene® LL-5102 LLDPE Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL-5102 makes for effici.. |
|||
Environmental Stress Crack Resistance | 250 hour | 250 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 8405 BK, 8405GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | 250 hour | 250 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 8405 UV8D, 8405G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | >= 250 hour @Temperature 50.0 °C |
>= 250 hour @Temperature 122 °F |
Igepal 100%; F20; ASTM D1693-B |
Borealis ME6032 Polypropylene ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. S.. |
|||
Environmental Stress Crack Resistance | >= 250 hour | >= 250 hour | 100% ant.; ASTM D1693-70 |
Total 49080 UV HDPE blow molding FINATHENE® 49080 UV is produced by the slurry loop low pressure polymerization process. FINATHENE® 49080 UV is a U.V.-stabilized, high molecular weight pelletized resin, intended for the productio.. |
|||
Environmental Stress Crack Resistance | >= 250 hour | >= 250 hour | F50, Anatarox 100%; ASTM D 1693B |
Total HDPE 56020 S XP High Density Polyethylene - Blow Molding HDPE 56020 S XP is a very high molecular weight (VHMW) high density polyethylene with a high resistance to impact, good chemical resistance and optimized balance between Environmental Stress Crack R.. |
|||
Environmental Stress Crack Resistance | >= 250 hour | >= 250 hour | ASTM D1693-70 |
Total ESD 201 B HDPE blow molding FINATHENE® ESD 201 B is a black conductive compound manufactured from high performance Finathene high density polyethylene. The use of this HDPE compound gives outstanding compatibility to (semi) h.. |
|||
Environmental Stress Crack Resistance | >= 250 hour | >= 250 hour | ASTM D1693-70 |
Total Finathene® SI 508 HDPE blow molding
(discontinued **) Finathene® SI 508 is part of a new generation of high density ethylene-hexene copolymers produced by the slurry loop low pressure polymerization process. Finathene® SI 508 is a high molecular weig.. |