Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 240 hour | 240 hour | Condition B, 10%; ASTM D1693 |
ExxonMobil LL 6407.67 Injection Molding Resin L Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processa.. |