Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 15.0 - 1000 hour @Temperature 50.0 - 60.0 °C |
15.0 - 1000 hour @Temperature 122 - 140 °F |
Average value: 240 hour Grade Count:20 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |